Old 26th July 2008, 06:42 PM   #1
Lew
(deceased)
 
Lew's Avatar
 
Join Date: Dec 2004
Location: East Coast USA
Posts: 3,191
Default

Ward

I sanded it again and used a weaker solution and I am definately seeing a wootz pattern starting to appear it shows swirls but seems low contrast it will need more coaxing.

Thanks

Lew
Lew is offline   Reply With Quote
Old 26th July 2008, 07:12 PM   #2
ward
Member
 
Join Date: Feb 2006
Posts: 637
Default

You always better off starting with a lower concentrate and just repeating coats over and over again
ward is offline   Reply With Quote
Old 26th July 2008, 08:27 PM   #3
Lew
(deceased)
 
Lew's Avatar
 
Join Date: Dec 2004
Location: East Coast USA
Posts: 3,191
Default

Here is a better pic you can see the pattern but it's not high contrast.
Attached Images
  
Lew is offline   Reply With Quote
Old 26th July 2008, 09:03 PM   #4
Atlantia
Member
 
Atlantia's Avatar
 
Join Date: Jun 2008
Location: The Sharp end
Posts: 2,928
Default

Another nice find Lew,
How are you etching it, dipping or painting on?
Would switching to citric acid now make any difference?
Atlantia is offline   Reply With Quote
Old 26th July 2008, 09:24 PM   #5
Lew
(deceased)
 
Lew's Avatar
 
Join Date: Dec 2004
Location: East Coast USA
Posts: 3,191
Default

Atlantia

I'm painting it on and I don't know if citric acid will do a good job on it?

Lew
Lew is offline   Reply With Quote
Old 26th July 2008, 09:47 PM   #6
ward
Member
 
Join Date: Feb 2006
Posts: 637
Default

if I may suggest more sanding got down to 2500 also still half your conentrate will take longer but will come out. you need to get rid of some pitting slow and sure. I think you should be able to get a decent pattern out of it. slow and sure. citric is not going to cut it on this tyoe of damascus. light etches neutralizing in between. you can use warm vinigar as last step
ward is offline   Reply With Quote
Old 26th July 2008, 10:48 PM   #7
Atlantia
Member
 
Atlantia's Avatar
 
Join Date: Jun 2008
Location: The Sharp end
Posts: 2,928
Default

I'm intrigued, I've never used ferric chloride.
I've always bathed as well, does it need to be mixed with a carrier to keep it on the blade? If not how do you stop it being patchy?
I like citric, mostly because its good and slow and idiot proof (an important factor for me! lol)
Which reminds me, Albanian? Wootz?
Have you guys mapped the geographical use of wootz? I wouldn't have even thought to check this dagger even though its a jambiya.

Cant wait to see the results on it!!

gene

P.S. I realise the blade must be a trade item.

Last edited by Atlantia; 27th July 2008 at 04:02 PM.
Atlantia is offline   Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 05:34 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.