Default Answer to my own question

Quote:
Originally Posted by Interested Party
Does anyone have any further experience/feedback/hearsay regarding Iron(III)sulfate? I.e. method of use, duration of contact with the surface to be etched, is it as messy and rust prone during cleaning as ferric chloride?
Rolland M had the answer to how to use sodium persulfate in a 2015 thread. "For pattern welded steel I preferably use sodium persulfate (fine etch crystal), 20 Gramm in 100 mL distilled water (~70°C ) with a pad, brush or Syringe." I hope this may help someone combing the archives one day for restoration information. Attached below is the entire thread.

http://www.vikingsword.com/vb/showth...ighlight=badek
Interested Party is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 08:36 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.