i recall from somewhere (?) that maille shirts would be put in a barrel with sand and rolled about to clean off rust, they were then oiled. possibly thus varnished with a drying oil that would inhibit rust. i recall olive oil was used by the romans. if used in thin coats, it does dry & form a protective coat.

i also recall reading about the maille used at omdurman being brittle due to age, rust and lack of maintenance.
kronckew is offline   Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 06:24 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.