Although I am not a metalurgist (spell?) I can speak to at least one point regarding pitting. Pitting startes either from specific acid concentration on one spot (like a drop of blood spatter on a blade) or on impurities in the metal that will oxidize quicker than the rest of the blade. Also, acidity varies from milimeter to milimeter in nature (for example in acidic soil). Even rusting or even patina comes from human intervention in some form or fashion (even in storage where patina may appear even).
Battara is offline  
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 05:00 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.