#3 |
|
Member
Join Date: Dec 2004
Posts: 1,712
|
Nice barung Spunjer!
Ive had the same expierience etching kukri, my conclusian was hot water & air promote an oxidisation that highlight the otherwise low contrast laminations, due to some layers or lamination lines of the bladel oxidising more rapidly than the others. As a technique I think of it as controled oxidisation highlighting. Guess it needs a heavy oil soaking afterwards. Spiral |
|
|
|
|
|