Quote:
Originally Posted by Interested Party
Does anyone have any further experience/feedback/hearsay regarding Iron(III)sulfate? I.e. method of use, duration of contact with the surface to be etched, is it as messy and rust prone during cleaning as ferric chloride?
|
Rolland M had the answer to how to use sodium persulfate in a 2015 thread.
"For pattern welded steel I preferably use sodium persulfate (fine etch crystal), 20 Gramm in 100 mL distilled water (~70°C ) with a pad, brush or Syringe." I hope this may help someone combing the archives one day for restoration information. Attached below is the entire thread.
http://www.vikingsword.com/vb/showth...ighlight=badek